  • 09-01-2025

    What are the most common defects encountered in aluminum welding?The most prevalent defects in aluminum welds typically include: - **Porosity** - **Cracking (Hot Cracking / Solidification Cracking)** - **Distortion** - **Lack of Fusion / Incomplete Penetration** - **Undercut / Bu
  • 07-30-2025

    1. What does "E71T" signify in flux-cored welding wire classifications?"E" indicates an electrode. "7" denotes a minimum tensile strength of 70,000 psi (70 ksi) in the as-welded condition. "1" indicates that the wire is suitable for all welding positions. "T" signifies a tubular or flux-cored electr
  • 07-30-2025

    1. What does "ER" signify in stainless steel welding wire classifications?"ER" stands for Electrode Rod, indicating a bare wire suitable for Gas Metal Arc Welding (GMAW or MIG) or Gas Tungsten Arc Welding (GTAW or TIG). This designation is standard across various metal types and is crucial for ident
  • Total 3 pages  Go to Page
  • Go

CONSULT YOUR GIANT WELDING EXPERT

We help you avoid the pitfalls to deliver the quality and value your welding wire need, on-time and on-budget.
Contact us
Products
About Us
Quick Links
Follow Us
COPYRIGHT © 2025 GIANT WELDING CO.,LTD ALL RIGHTS RESERVED.